Polymer Property : Tensile Stress = 17.24 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 17.24 MPa

@Strain 38.84 %,
Temperature 60.0 °C
2500 psi

@Strain 38.84 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers
Tensile Stress 17.24 MPa

@Strain 1.23 %,
Temperature 23.0 °C
2500 psi

@Strain 1.23 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..