Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.74 MPa @Strain 100 %, Temperature 23.0 °C |
252 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE) Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 .. |
|||
Tensile Stress | 1.74 MPa @Strain 100 % |
252 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P1955 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.74 MPa @Strain 300 % |
252 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3940C TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.74 MPa @Strain 8.52 %, Temperature 23.0 °C |
252 psi @Strain 8.52 %, Temperature 73.4 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 1.74 MPa @Strain 8.52 %, Temperature 23.0 °C |
252 psi @Strain 8.52 %, Temperature 73.4 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |