Polymer Property : Tensile Stress = 1.30 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.30 MPa

@Strain 100 %
189 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S KG 40A-3S2016 Thermoplastic Elastomer (TPE)
OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tensile Stress 1.30 MPa

@Strain 100 %
189 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® N8950 TPE, Nylon Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se..
Tensile Stress 1.30 MPa

@Strain 100 %
189 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3850H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.30 MPa

@Strain 100 %
189 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P52-004A-3B TPE, PP Overmold or Standalone use
Characteristics: Soft, flexible feelExcellent grip characteristicsGood weatherabilityGood compression setEasy processability and colorabilityAvailable FDA and medical gradesAvailable translucent gra..
Tensile Stress 1.30 MPa

@Strain 5.00 %,
Temperature 100 °C
189 psi

@Strain 5.00 %,
Temperature 212 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET  (Unverified Data**)
Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio..
Tensile Stress 1.30 MPa

@Strain 100 %
189 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G45A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 1.30 MPa

@Strain 100 %
189 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G45A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G45A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..