Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.850 MPa @Strain 6.36 %, Temperature 120 °C |
123 psi @Strain 6.36 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 0.850 MPa @Strain 0.110 %, Temperature 40.0 °C |
123 psi @Strain 0.110 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |