Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.580 MPa @Strain 100 % |
84.1 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3930CT TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 0.580 MPa @Strain 0.0600 %, Temperature 23.0 °C |
84.1 psi @Strain 0.0600 %, Temperature 73.4 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET