Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 84.0 GPa @Temperature 300 °C |
12200 ksi @Temperature 572 °F |
|
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us.. |
|||
Modulus of Elasticity | 84.2 GPa @Temperature 204 °C |
12200 ksi @Temperature 399 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 705 Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other .. |