Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 78.0 GPa @Temperature 150 °C |
>= 11300 ksi @Temperature 302 °F |
|
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Modulus of Elasticity | 77.8 GPa @Temperature 316 °C |
11300 ksi @Temperature 601 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 705 Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other .. |