Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 77.0 GPa @Temperature 150 °C |
>= 11200 ksi @Temperature 302 °F |
|
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Modulus of Elasticity | >= 77.0 GPa @Temperature 20.0 °C |
>= 11200 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Modulus of Elasticity | >= 77.0 GPa @Temperature 20.0 °C |
>= 11200 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |