Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 236 GPa @Temperature 20.0 °C |
34200 ksi @Temperature 68.0 °F |
|
Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel Description: Uddeholm Vancron 40 is a nitrided powder tool steel, which means that a “surface coating” is already integrated into the finished tooling material. The result is a tool surface with v.. |