Mechanical Properties Metric English Comments
Modulus of Elasticity 211 GPa

@Temperature 100 °C
30600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Modulus of Elasticity 211 GPa

@Temperature 100 °C
30600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 211 GPa

@Temperature 100 °C
30600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Modulus of Elasticity 211 GPa

@Temperature 100 °C
30600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Modulus of Elasticity 211 GPa

@Temperature 100 °C
30600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Modulus of Elasticity 211 GPa

@Temperature 200 °C
30600 ksi

@Temperature 392 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Modulus of Elasticity 211 GPa

@Temperature 100 °C
30600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..
Modulus of Elasticity 211 GPa

@Temperature 100 °C
30600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..
Modulus of Elasticity 211 GPa

@Temperature 20.0 °C
30600 ksi

@Temperature 68.0 °F
Dynamic
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..