Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 427 °C |
25700 ksi @Temperature 801 °F |
|
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 427 °C |
25700 ksi @Temperature 801 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 427 °C |
25700 ksi @Temperature 801 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 427 °C |
25700 ksi @Temperature 801 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 427 °C |
25700 ksi @Temperature 801 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 427 °C |
25700 ksi @Temperature 801 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 427 °C |
25700 ksi @Temperature 801 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 399 °C |
25700 ksi @Temperature 750 °F |
|
EDRO #7 Shock Resistant S7 Tool Steel EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 427 °C |
25700 ksi @Temperature 801 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Modulus of Elasticity | 177 GPa @Temperature 538 °C |
25700 ksi @Temperature 1000 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |