Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, gas tungsten arc welded Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged at 649°C (1200°F) for 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged 1300 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, weld metal, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, weld metal, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, weld metal, aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 600 °C |
25200 ksi @Temperature 1110 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 1000 °C |
25300 ksi @Temperature 1830 °F |
|
Latrobe CBS-223â„¢ VIM-VAR Carburizing Bearing and Gear Steel CBS-223 VIM-VAR steel is a double vacuum melted carburizing steel with high hot hardness characteristics. Double vacuum melting sequentially combines vacuum induction melting with VACARCâ„¢ remel.. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Modulus of Elasticity | 174 GPa @Temperature 649 °C |
25200 ksi @Temperature 1200 °F |
Heat treated at 1066°C, air cooled |
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Modulus of Elasticity | 174 GPa @Temperature 316 °C |
25200 ksi @Temperature 601 °F |
|
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-.. |