Mechanical Properties Metric English Comments
Izod Impact, Notched 0.230 J/cm

@Temperature -30.0 °C
0.431 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® INP562 ABS
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Izod Impact, Notched 0.230 J/cm

@Temperature 23.0 °C
0.431 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® INP581 ABS
High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for..
Izod Impact, Notched 0.230 J/cm

@Temperature -30.0 °C
0.431 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy FXTW26SK ASA
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.230 J/cm

@Temperature -30.0 °C
0.431 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific)
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region...
Izod Impact, Notched 0.230 J/cm

@Temperature -30.0 °C
0.431 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East)
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
Copyright © lookpolymers.com All Rights Reserved