Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy) Custom MoldingInformation provided by PolyOne |
|||
Izod Impact, Notched | 9.60 J/cm @Temperature 23.0 °C |
18.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa.. |