Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 4.61 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 8.63 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL TE5109 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.61 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
8.63 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 4.61 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 8.63 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL TE5104 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.61 J/cm @Thickness 3.20 mm |
8.63 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron SE45I Extrusion ABS Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Izod Impact, Notched | 4.61 J/cm @Thickness 3.20 mm |
8.63 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron SE45I Extrusion ABS Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali |