Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.22 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
7.90 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI100 ABS, High Impact Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
7.90 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI100H ABS, High Impact, High Toughness Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
7.90 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
7.90 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical SH610A ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
7.90 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8010 Availability: North AmericaForms: PelletsProcessing Method: Extrusion Blow Molding and Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 6.35 mm |
7.90 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
7.90 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 6.35 mm |
7.90 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.22 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
7.90 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |