Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.3333 J/cm @Thickness 3.20 mm |
6.2446 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Izod Impact, Notched | 3.3333 J/cm @Thickness 3.20 mm |
6.2446 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |