Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.24 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
6.06 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 3.24 J/cm @Temperature 23.0 °C |
6.06 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H1000PWI High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weathering, reduce heat conductivity to waterRecommended Applications: Above ground pipes, double wall pipesInforma.. |
|||
Izod Impact, Notched | 3.24 J/cm @Temperature 23.0 °C |
6.06 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LA50 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 3.24 J/cm @Temperature -30.0 °C |
6.06 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LA50 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 3.24 J/cm @Temperature 23.0 °C |
6.06 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LA60 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 3.24 J/cm @Temperature -30.0 °C |
6.06 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LA60 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 3.24 J/cm @Temperature 23.0 °C |
6.06 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LB40 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 3.24 J/cm @Temperature -30.0 °C |
6.06 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LB40 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |