Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.440 J/cm @Thickness 3.17 mm |
0.824 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical MI-730 MIPS |
|||
Izod Impact, Notched | 0.440 J/cm @Thickness 6.35 mm |
0.824 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical MI-750 MIPS Medium impact |
|||
Izod Impact, Notched | 0.440 J/cm @Temperature -40.0 °C |
0.824 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman DuraStar DS1900HF Polymer, Natural Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur.. |
|||
Izod Impact, Notched | 0.440 J/cm @Temperature -40.0 °C |
0.824 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman DuraStar DS1910HF Polymer, Natural Durastar DS1910HF polymer is a high flow grade of Durastar that contains a mold release. Durastar DS1910HF flow lengths are increased 20-40% relative to Durastar DS1010 as shown by spiral flow testi.. |
|||
Izod Impact, Notched | 0.440 J/cm @Temperature -40.0 °C |
0.824 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Izod Impact, Notched | 0.440 J/cm @Temperature -40.0 °C |
0.824 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman DuraStar MN631 Polymer, Natural Durastar Polymer MN631 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Izod Impact, Notched | 0.440 J/cm @Temperature -40.0 °C |
0.824 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar AN011 Copolyester Eastar AN011 copolyester is a high flow product. Eastar AN011 flow lengths are increased 20-40% relative to Eastar AN001 as shown by spiral flow testing. Other outstanding features of Eastar are eas.. |
|||
Izod Impact, Notched | 0.440 J/cm @Temperature -40.0 °C |
0.824 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar AN014 Copolyester Eastar AN014 copolyester is a high flow product that contains a mold release. Eastar AN014 flow lengths are increased 20-40% relative to Eastar AN004 as shown by spiral flow testing. Other outstandi.. |