Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-40006T/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-40006T/4 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-40009.5S/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-40012T/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-40036S/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-40054V/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-40406B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-40810B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-41014B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-42424B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-43036B Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-80036S/2 Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |
|||
Heat Seal Strength | 3.00 - 9.23 g/25 mm | 0.00661 - 0.0204 lb/in | Transverse Direction; ASTM-D882 |
Caplinq LINQSTAT™ VCF-40054V/m Product Description: LINQSTAT™ VCF-Series is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electroni.. |