Polymer Property : Impact Test = 20.7 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific)
Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied..
Impact Test 28.0 J

@Temperature -40.0 °C
20.7 ft-lb

@Temperature -40.0 °F
Instrumented, 15 mph; ASTM 3763
Phillips Sumika Marlex® CHP-015 Thermoplastic Polyolefin  (discontinued **)
Applications: Driver-side air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 201..
Impact Test 28.0 J

@Temperature -29.0 °C
20.7 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
LyondellBasell Pro-fax 7523 Polypropylene Impact Copolymer
Primary Processing Method: Injection MoldingKey Features: good cold impact resistance, good stiffness and impact balance, excellent dimensional stability, FDA acceptableApplications: seating, applia..
Impact Test 28.0 J

@Temperature -29.0 °C
20.7 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
LyondellBasell Pro-fax 7624 Polypropylene Impact Copolymer, Heat- and Extraction-Resistant
Primary Processing Method: Injection MoldingKey Features: resistant to aging at high temperatures in both wet and dry environments, good cold impact resistance, excellent dimensional stability, FDA ..
Impact Test 28.0 J
20.7 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 1110FV PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I..
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 1110R PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 1110V PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region.
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem HATX200 PEI+PCE
High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli..
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli..
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli..
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 28.0 J
20.7 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DX91077 PC
LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified.
Impact Test 28.0 J

@Temperature 23.0 °C
20.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..