Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 18.0 J | 13.2 ft-lb | Rheometric |
DuPont Bexloy® AXW502NC010 Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |