Polymer Property : 300% Modulus = 1.96 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00860 - 0.0135 GPa
1.25 - 1.96 ksi
Cure: 40 mins at 135°C; ISO 37
Kraton® Cariflex™ IR0307 K Polyisoprene
Description: Cariflex IR0307 KU polymer is a solution polymerized polyisoprene with a high cis-1,4 content. It has a high molecular weight as indicated by its Logarithmic Inherent Viscosity (LIV) va..
300% Modulus 0.00860 - 0.0135 GPa
1.25 - 1.96 ksi
Cure: 40 mins at 135°C; ISO 37
Kraton® IR307 Polyisoprene
Description: Kraton IR307 polymer is a solution polymerized polyisoprene with a high cis-1,4 content. It has a high molecular weight as indicated by its limiting viscosity number of 7.75 dl/g. Regi..