Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00300 - 0.00600 GPa | 0.435 - 0.870 ksi | ASTM D 638 |
API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |