Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.01606 GPa | 2.329 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Hi-Sil 243 LD Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.01606 GPa | 2.329 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 91A MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.01606 GPa | 2.329 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Hi-Sil 243 LD Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.01606 GPa | 2.329 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 91A MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |