Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0118 GPa | 1.71 ksi | Cured |
KKPC Kumho KHS 68 High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
300% Modulus | 0.0118 GPa | 1.71 ksi | |
Taiwan PU Corporation TPU-B95 General Grade, Blow Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0118 GPa | 1.71 ksi | |
Taiwan PU Corporation TPU-BH95 Hydrolysis Resistance, Blow Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0118 GPa | 1.71 ksi | |
Taiwan PU Corporation TPU-C95 General Grade, Calender Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0118 GPa | 1.71 ksi | |
Taiwan PU Corporation TPU-CH95 High Hydrolysis Resistance, Calender Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0118 GPa | 1.71 ksi | |
Taiwan PU Corporation TPUI-E90 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0118 GPa | 1.71 ksi | |
Taiwan PU Corporation TPUI-L85 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
300% Modulus | 0.0118 GPa | 1.71 ksi | |
Taiwan Sheen Soon Sheenthane® A8550 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0118 GPa | 1.71 ksi | |
Taiwan Sheen Soon Sheenthane® A8630F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0118 GPa | 1.71 ksi | |
Taiwan Sheen Soon Sheenthane® A9200B Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionHalogen-free fire-retardant gradeInformation provided by Taiwan Sheen Soon Co., LTD. |