Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0101 GPa | 1.46 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0101 GPa | 1.46 ksi | Injection molded parts; ISO 37 |
Huntsman IROGRAN® A 80 H 4826 TPU-Polyester Introduction: IROGRAN A 80 H 4826 is a thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of this product are excellent mechanical properties and hig.. |
|||
300% Modulus | 0.0101 GPa | 1.46 ksi | ASTM D412 |
UBE UBEPOL BR100 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
300% Modulus | 0.0101 GPa | 1.46 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.0101 GPa | 1.46 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 Dense Extruded Profile FormulationNordel® IP 4570 |
|||
300% Modulus | 0.0101 GPa | 1.46 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 General Purpose Compound FormulationNordel® IP 4570 |