Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00250 GPa | 0.363 ksi | ASTM D412 |
Polimeri Europa Europrene® SOL T 161C Styrene - Butadiene Block Copolymer Europrene® SOL T 161C is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. A non-staining antioxidant .. |
|||
300% Modulus | 0.00250 GPa | 0.363 ksi | ASTM D412 |
Polimeri Europa Europrene® SOL T 166 Styrene - Butadiene Block Copolymer Europrene® SOL T 166 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. A non-staining antioxidant s.. |
|||
300% Modulus | 0.00250 GPa | 0.363 ksi | ASTM D412 |
Polimeri Europa Europrene® SOL T 6302 Styrene - Butadiene Block Copolymer Europrene® SOL T 6302 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. A non-staining antioxidant .. |
|||
300% Modulus | 0.00250 GPa | 0.363 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z506 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
300% Modulus | 0.00250 GPa | 0.363 ksi | ISO 37 |
Kraton® D1184 A (SBS) Branched Block Copolymer Description: Kraton D1184 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
300% Modulus | 0.00250 GPa | 0.363 ksi | ISO 37 |
Kraton® D1184 E (SBS) Branched Block Copolymer Description: Kraton D1184 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
300% Modulus | 0.00250 GPa | 0.363 ksi | Measured on injection molded slab; ISO 37 |
Kraton® D4153 E (O/E SBS) Linear Block Copolymer Description: Kraton D4153 E is an oil-extended linear block copolymer based on styrene and butadiene with bound styrene in the neat polymer of 35% mass. It contains 40 phr paraffinic oil which is cl.. |
|||
300% Modulus | 0.00250 GPa @Time 7200 sec |
0.363 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-55-1000 TPE Product Description: StarXTRUDE XTR-55-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |
|||
300% Modulus | 0.00250 GPa @Temperature 23.0 °C |
0.363 ksi @Temperature 73.4 °F |
12 months, Weathering @ 45° South, 25 mil - Natural, Ohio |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
300% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Precipitated Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.00250 - 0.00900 GPa | 0.363 - 1.31 ksi | ASTM D 638 |
API Megol AM DP2339 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
300% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Precipitated Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.00250 GPa | 0.363 ksi | ASTM D412 |
Polimeri Europa Europrene® SOL T 161B Styrene - Butadiene Block Copolymer Europrene® SOL T 161B is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. A non-staining antioxidant .. |
|||
300% Modulus | 0.00250 GPa @Time 7200 sec |
0.363 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7155-1000 TPE Product Description: StarFlex P 7155-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |