Mechanical Properties Metric English Comments
300% Modulus 0.0130 - 0.0190 GPa
1.89 - 2.76 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1500 Styrene Butadiene Rubber
KRALEX® 1500 is a standard grade of styrene butadiene rubber. It is produced by a technology of cold emulsion polymerization based on soaps of rosin acids and contains 23.5% of chemically bonded ..
300% Modulus 0.0140 - 0.0190 GPa
2.03 - 2.76 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1706 Styrene Butadiene Rubber
KRALEX® 1706 is a standard grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5..
Copyright © lookpolymers.com All Rights Reserved