Polymer Property : 300% Modulus = 0.0235 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0235 GPa
3.41 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Vul-Cup 40KE Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.0235 GPa
3.41 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Vul-Cup 40KE Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..