Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00900 GPa | 1.31 ksi | 0.025" extruded film; DIN 53504 |
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti.. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane Type : Pearlthane® D91T80 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
300% Modulus | 0.00900 GPa | 1.30 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO D12T80 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T80 is a high performance bio-based thermoplastic polyurethane. With ca. 42% bio-based content.Main Application : Injection MouldingSpecial Features : Properties similar.. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | DIN 53504 |
Lubrizol ESTANE® T5090 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1180 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2185 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412; ASTM D638 |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1680AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412/D638 |
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin .. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D638 |
ELASTO UK Dryflex® 420401S SBS Based Material, 40D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D638 |
ELASTO UK Dryflex® 422401S SBS Based Material, 40D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 General Purpose Compound FormulationNordel® IP 4640 |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770P Dense Extruded Profile FormulationNordel® IP 4770P |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4770R Dense Extruded Profile FormulationNordel® IP 4770R |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412/D638 |
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane Features: It has the highest heat resistance of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and b.. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | DIN 53504 |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | DIN 53504 |
Lubrizol ESTANE® 58214 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
300% Modulus | 0.00900 GPa | 1.31 ksi | DIN 53504 |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |