Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00683 GPa | 0.990 ksi | ASTM D412 |
Teknor Apex TEKRON® 4300-B88 2UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00683 GPa | 0.990 ksi | ASTM D412 |
Teknor Apex TEKRON® 4300-B88 UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00683 GPa | 0.990 ksi | ASTM D412 |
Teknor Apex TEKRON® 4300-D90A Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00683 GPa | 0.990 ksi | ASTM D412 |
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00683 GPa | 0.991 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-774 (SRF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.00683 GPa | 0.991 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-774 (SRF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |