Mechanical Properties Metric English Comments
300% Modulus 0.00248 GPa
0.360 ksi
Typical properties on film cast from toluene solution; ASTM D412
Kraton® D1126 P (SIS) Radial Copolymer
Description: Kraton D1126 P is a clear, radial copolymer based on styrene and isoprene, with a polystyrene content of 21%. In addition, it has a diblock content of 30% and high melt flow. It is supp..
300% Modulus 0.00248 GPa
0.360 ksi
ASTM D 412
CPT C-Flex® R70-072 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..