Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00120 GPa | 0.174 ksi | ASTM D412 |
Multibase Multi-Flex® TPE A 7101 BLK Ash is 36.2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
300% Modulus | 0.00120 GPa | 0.174 ksi | Measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D1118 K (SBS) Diblock Copolymer Description: Kraton D1118 K is a clear, diblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from North America in the physical form identified: Kraton .. |
|||
300% Modulus | 0.00120 GPa | 0.174 ksi | ASTM D-412 |
Dynasol Solprene® 4318 Thermoplastic Rubber SBS Dry Solprene 4318 is a linear block copolymer of styrene and butadiene, having 32% of styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a .. |