Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 3770 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 24.0 - 26.0 MPa
3480 - 3770 psi
Mild steel, Shear
Permabond TA4310 Toughened Acrylic Adhesive
PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue...
Copyright © lookpolymers.com All Rights Reserved