Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 19.0 MPa | 2750 psi | |
Resin Technology Group 345 General Purpose Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 345 General Purpose Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Adhesive Bond Strength | 19.0 MPa | 2750 psi | alum/aluminum |
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any .. |
|||
Adhesive Bond Strength | 19.0 MPa | 2750 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon Epoxy Plusâ„¢ 25 Grey Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 19.0 MPa | 2750 psi | Grit blasted steel |
Loctite® Super Bonder® 495 Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Adhesive Bond Strength | >= 19.0 MPa | >= 2750 psi | ASTM D4541 |
Chesterton ARC 982 100% Novolac acid resistant coating Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo.. |
|||
Adhesive Bond Strength | 19.0 MPa @Temperature 82.2 °C |
2750 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-1/A Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Adhesive Bond Strength | 19.0 MPa @Temperature 25.0 °C |
2750 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-31 Epoxy Adhesive Is a neutral-colored thixotropic paste material having a creamy or buttery consistency that will not flow even when cured at elevated temperatures A-31 also features Extremely low outgassing charact.. |