Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 16.38 MPa | 2375 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Combo Wear FC Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 16.38 MPa | 2375 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Wear Guard (Fine Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Adhesive Bond Strength | 16.38 MPa | 2375 psi | Adhesive tensile shear strength; ASTM D1002 |
Devcon Wear Guard (High Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |