Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | Steel, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | 20.0 - 22.0 MPa | 2900 - 3190 psi | Brass, Shear; ISO 4587 |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Adhesive Bond Strength | 20.0 - 22.0 MPa | 2900 - 3190 psi | Stainless Steel, Shear; ISO 4587 |
Permabond 170 Cyanoacrylate, gap filling PERMABOND® 170 is a methyl cyanoacrylate adhesive. It is a single part, high viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. Permabond 170 w.. |
|||
Adhesive Bond Strength | 20.0 - 22.0 MPa | 2900 - 3190 psi | Steel, Shear; ISO 4587 |
Permabond 268 Cyanoacrylate, General purpose PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano.. |
|||
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | ISO 4587, Shear |
Permabond 790 Cyanoacrylate, Surface insensitive PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Adhesive Bond Strength | 20.0 - 22.0 MPa | 2900 - 3190 psi | Mild steel, Shear |
Permabond TA4300 Toughened Acrylic Adhesive PERMABOND® TA4300 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Adhesive Bond Strength | 20.0 - 22.0 MPa | 2900 - 3190 psi | Steel, Shear; ISO 4587 |
Permabond 108 Cyanoacrylate, gap filling PERMABOND® 108 is an intermediate viscosity cyanoacrylate that is used to bond through intermediate gaps. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate adhes.. |
|||
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | ISO 4587, Shear |
Permabond 791 Cyanoacrylate, Surface insensitive PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | Steel, Shear; ISO 4587 |
Permabond 795 Cyanoacrylate, Surface insensitive PERMABOND® 795 is a moderate viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastome.. |
|||
Adhesive Bond Strength | 20.0 - 22.0 MPa | 2900 - 3190 psi | Steel, Shear; ISO 4587 |
Permabond 799 Cyanoacrylate, Surface insensitive PERMABOND® 799 is a high viscosity cyanoacrylate that combines fast cure with the ability to cure through a large gap. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cu.. |
|||
Adhesive Bond Strength | 20.0 - 22.0 MPa | 2900 - 3190 psi | Steel, Shear; ISO 4587 |
Permabond 919 Cyanoacrylate, High temperature Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I.. |
|||
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | ISO 4587, Shear |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |