Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 18.0 MPa | 2610 psi | Tensile Shear Strength; ASTM D1002 |
Protective Coating PC-SuperEpoxy™ Translucent Epoxy Putty PC-SUPEREPOXY™ is a non-drip, thixotropic, translucent paste with unlimited uses in bonding, sealing, and as a filler for most materials. Unlike conventional liquid epoxies, PC-SUPEREPOXY™ can be.. |
|||
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | Steel, Shear; ISO 4587 |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | ISO 4587, Shear |
Permabond 790 Cyanoacrylate, Surface insensitive PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Adhesive Bond Strength | 18.0 - 21.0 MPa | 2610 - 3050 psi | Mild steel, Shear |
Permabond ET505 Epoxy Resin PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | ISO 4587, Shear |
Permabond 791 Cyanoacrylate, Surface insensitive PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | Steel, Shear; ISO 4587 |
Permabond 795 Cyanoacrylate, Surface insensitive PERMABOND® 795 is a moderate viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastome.. |
|||
Adhesive Bond Strength | 18.0 - 20.0 MPa | 2610 - 2900 psi | Mild steel, Shear |
Permabond ET538 Epoxy Resin PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia.. |
|||
Adhesive Bond Strength | 18.0 - 22.0 MPa | 2610 - 3190 psi | ISO 4587, Shear |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Adhesive Bond Strength | 18.0 - 20.0 MPa | 2610 - 2900 psi | Mild steel, Shear |
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |