Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.1101 GPa | 15.97 ksi | ASTM D790 |
Dow Engage® 8445 Polyolefin Elastomer Description: Engage® 8445 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p.. |