Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.862 GPa | 125 ksi | Crosshead speed - 0.5" min; ASTM D790 |
LyondellBasell Alathon® ETP H4745 High Density Polyethylene ApplicationsALATHON H 4745 is a new, multi-purpose, high-flow resin featuring enhanced cold temperature impact performance, enhanced processability and thermal stability for fast cycling and exhibit.. |
|||
2% Secant Modulus | 0.862 GPa | 125 ksi | Crosshead speed - 0.5" min; ASTM D790 |
LyondellBasell Alathon® ETP H4837 High Density Polyethylene ApplicationsALATHON H 4837 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processability and thermal stability, with good color a.. |