Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 7.00 J | 5.16 ft-lb | |
Haynes 625 alloy, plate after 1000 hours at 760°C (1400°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Charpy Impact | 7.00 J | 5.16 ft-lb | |
Haynes 625 alloy, plate after 8000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Charpy Impact | 7.00 J | 5.16 ft-lb | |
Haynes 625 alloy, plate after 8000 hours at 760°C (1400°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Charpy Impact | 7.00 - 15.0 J | 5.16 - 11.1 ft-lb | Notched; after age hardening |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |
|||
Charpy Impact | 7.00 J @Temperature -196 °C |
5.16 ft-lb @Temperature -321 °F |
V-notch |
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |