Charpy Impact >= 60.0 J

@Temperature 0.000 °C
>= 44.3 ft-lb

@Temperature 32.0 °F
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness
Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist..
Charpy Impact >= 60.0 J

@Temperature -196 °C
>= 44.3 ft-lb

@Temperature -321 °F
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42
Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0...
Charpy Impact 60.0 J
44.3 ft-lb
Guaranteed in L Direction
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel
Description: Virgo 39 is a 16% Cr, 5% Ni, 1% Mo low carbon martensitic stainless steel. The grade is specially designed to combine high mechanical properties including toughness and improved corrosi..
Charpy Impact 60.0 J
44.3 ft-lb
V-Notch; 5.25 in. Test Specimen
Latrobe Lescalloy® 410Cb High Strength Stainless Steel
LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe..
Charpy Impact 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
Haynes Ultimet® alloy, aged 1000 hours at 982°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 60.0 J
44.3 ft-lb
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Charpy Impact 60.0 J
44.3 ft-lb
Longitudinal, (10mmx10mm)
Bisalloy Steels BisPlate 320 Thickness >80-100 mm
A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Deflector Plates, Chutes, Storage Bins, Dump Truck Liners, Earthm..
Charpy Impact 60.0 J
44.3 ft-lb
Longitudinal, (10mmx10mm)
Bisalloy Steels BisPlate 320 Thickness 16-80 mm
A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Deflector Plates, Chutes, Storage Bins, Dump Truck Liners, Earthm..
Charpy Impact 60.0 J
44.3 ft-lb
Longitudinal, (10mmx10mm)
Bisalloy Steels BisPlate 320 Thickness 5 -
A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Deflector Plates, Chutes, Storage Bins, Dump Truck Liners, Earthm..
Copyright © lookpolymers.com All Rights Reserved