Mechanical Properties Metric English Comments
Charpy Impact 55.0 J
40.6 ft-lb
V notch. Short transverse direction. 200°C tempering temperature (2 + 2h).
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..
Charpy Impact 55.0 J

@Temperature 100 °C
40.6 ft-lb

@Temperature 212 °F
V-notch. Short transverse direction. 45 HRC
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..
Charpy Impact 55.0 J
40.6 ft-lb
Longitudinal, (10mmx10mm)
Bisalloy Steels BisPlate 400 Thickness >80-100 mm
A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea..
Charpy Impact 55.0 J
40.6 ft-lb
Longitudinal, (10mmx10mm)
Bisalloy Steels BisPlate 400 Thickness 5 -
A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea..
Charpy Impact 55.0 J

@Temperature -20.0 °C
40.6 ft-lb

@Temperature -4.00 °F
Transverse
Bisalloy Steels BisPlate 80PV Thickness >80-100 mm
A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage ..
Charpy Impact 55.0 J

@Temperature -20.0 °C
40.6 ft-lb

@Temperature -4.00 °F
Transverse
Bisalloy Steels BisPlate 80PV Thickness 6-
A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage ..
Charpy Impact 55.0 J
40.6 ft-lb
Longitudinal, (10mmx10mm)
Bisalloy Steels BisPlate 400 Thickness 16-80 mm
A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea..
Charpy Impact 55.0 J

@Temperature -20.0 °C
40.6 ft-lb

@Temperature -4.00 °F
Transverse
Bisalloy Steels BisPlate 80PV Thickness 16-80 mm
A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage ..
Charpy Impact 55.0 J

@Temperature -54.0 °C
40.6 ft-lb

@Temperature -65.2 °F
V-notch
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties
Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to..
Copyright © lookpolymers.com All Rights Reserved