Mechanical Properties Metric English Comments
Charpy Impact 250 J

@Temperature -196 °C
184 ft-lb

@Temperature -321 °F
Typical
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel
Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water ..
Charpy Impact 250 J

@Temperature -196 °C
184 ft-lb

@Temperature -321 °F
Typical
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel
Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi..
Charpy Impact 250 J
184 ft-lb
Typical
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel
Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k..