Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 175 J @Temperature -196 °C |
129 ft-lb @Temperature -321 °F |
Typical |
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
Charpy Impact | 175 J | 129 ft-lb | Typical |
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, 1149°C (2100°F) Solution Treated, UNS N06601 Allegheny Ludlum's AL 601 alloy is an austenitic nickel-chromium-iron alloy designed for both heat and corrosion resistance. As compared to AL 600 alloy, the AL 601 alloy has, in addition to increa.. |