Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 15.0 J | 11.1 ft-lb | Typical (Transverse) |
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. T.. |
|||
Charpy Impact | 15.0 J @Temperature -20.0 °C |
11.1 ft-lb @Temperature -4.00 °F |
Typical (Longitudinal) |
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. T.. |
|||
Charpy Impact | 15.0 J | 11.1 ft-lb | |
Industeel Superplast® 350 Mold Steel SUPERPLAST® 350 offers improved machinability, improved consistency and weldability, improved thermal conductivity, with a higher hardness allowing better mechanical properties and polishability... |
|||
Charpy Impact | 15.0 J | 11.1 ft-lb | |
Haynes 625 alloy, plate after 1000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Charpy Impact | 15.0 J | 11.1 ft-lb | |
Haynes 625 alloy, plate after 4000 hours at 870°C (1600°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Charpy Impact | 15.0 J | 11.1 ft-lb | 50% cold rolled and 500 hours at 500°C (930°F) |
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Charpy Impact | 15.0 J @Temperature -40.0 °C |
11.1 ft-lb @Temperature -40.0 °F |
Transverse |
ThyssenKrupp SECURE 500 Structural Steel This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 500 for civil use, that is usually produced in thickness from 3 mm up to 90 mm.App.. |
|||
Charpy Impact | 15.0 J @Temperature -40.0 °C |
11.1 ft-lb @Temperature -40.0 °F |
Transverse |
ThyssenKrupp SECURE 600 Structural Steel This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 600 for civil use, that is usually produced from 4 up to 40 mm in thickness.Applic.. |
|||
Charpy Impact | 15.0 J | 11.1 ft-lb | tempering at 450°C (842°F). Hardened at 960°C (1760°F). Quenched in air. Tempered twice. |
Assab Steels CALMAX Plastic Mold Material CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo.. |