Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 60.0 J @Temperature 0.000 °C |
>= 44.3 ft-lb @Temperature 32.0 °F |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Charpy Impact | >= 60.0 J @Temperature -196 °C |
>= 44.3 ft-lb @Temperature -321 °F |
|
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42 Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0... |
|||
Charpy Impact | 60.0 J | 44.3 ft-lb | Guaranteed in L Direction |
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel Description: Virgo 39 is a 16% Cr, 5% Ni, 1% Mo low carbon martensitic stainless steel. The grade is specially designed to combine high mechanical properties including toughness and improved corrosi.. |
|||
Charpy Impact | 60.0 J | 44.3 ft-lb | V-Notch; 5.25 in. Test Specimen |
Latrobe Lescalloy® 410Cb High Strength Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
Charpy Impact | 60.0 J @Temperature 23.0 °C |
44.3 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, aged 1000 hours at 982°C Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 60.0 J | 44.3 ft-lb | |
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Charpy Impact | 60.0 J | 44.3 ft-lb | Longitudinal, (10mmx10mm) |
Bisalloy Steels BisPlate 320 Thickness >80-100 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Deflector Plates, Chutes, Storage Bins, Dump Truck Liners, Earthm.. |
|||
Charpy Impact | 60.0 J | 44.3 ft-lb | Longitudinal, (10mmx10mm) |
Bisalloy Steels BisPlate 320 Thickness 16-80 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Deflector Plates, Chutes, Storage Bins, Dump Truck Liners, Earthm.. |
|||
Charpy Impact | 60.0 J | 44.3 ft-lb | Longitudinal, (10mmx10mm) |
Bisalloy Steels BisPlate 320 Thickness 5 - A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Deflector Plates, Chutes, Storage Bins, Dump Truck Liners, Earthm.. |