Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 33.9 J | 25.0 ft-lb | 496°C Temper Temperature |
Latrobe Lescalloy® 16NCD13 VAC-ARC High Strength Alloy Steel 16NCD13 VAC-ARC is a premium quality low alloy, carburizing casehardenable vacuum arc remelted steel which takes its name from the French industry designation. In the carburized condition, its high .. |
|||
Charpy Impact | 33.9 J | 25.0 ft-lb | V-Notch; Air Cooled from 1010°C; 172°C Temper Temperature |
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12) TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste.. |
|||
Charpy Impact | 33.9 J | 25.0 ft-lb | V-Notch; Air Cooled from 1010°C; 370 Temper Temperature |
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11) TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides.. |
|||
Charpy Impact | 33.9 J | 25.0 ft-lb | V-Notch |
ECOMold 135 Copper Mold Material ECOMold® copper alloys (beryllium-free) are engineered specifically for plastics industry applications. ECOMold® 135 has superior thermal conductivity compared to other common mold materials. T.. |
|||
Charpy Impact | 33.9 J @Temperature 20.0 °C |
25.0 ft-lb @Temperature 68.0 °F |
Age hardened at 42 HRC |
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, .. |
|||
Charpy Impact | 33.9 J @Temperature 20.0 °C |
25.0 ft-lb @Temperature 68.0 °F |
Age hardened at 42 HRC |
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, unifor.. |
|||
Charpy Impact | >= 33.9 J @Thickness >=3.17 mm |
>= 25.0 ft-lb @Thickness >=0.125 in |
transverse |
American Utility Metals 3CR12® Stainless Steel 3CR12 is a weldable ferritic stainless steel, specifically designed for aggressive material handling applications. It is intended to provide the benefits of traditional stainless steel, such as stre.. |
|||
Charpy Impact | 33.9 J | 25.0 ft-lb | Notched; at 38 HRC |
Schmolz + Bickenbach Formadur® PH X Superclean Plastic Mold Steel Description: Formadur® PH X Superclean is a corrosion-resistant, martensitic precipitation hardened stainless steelCharacteristics: Excellent resistance to corrosion; Excellent polishability; Excel.. |