Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 127 J @Temperature 23.0 °C |
93.7 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 127 J @Temperature 23.0 °C |
93.7 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 127 J @Temperature 23.0 °C |
93.7 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 127 J @Temperature 23.0 °C |
93.7 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 127 J @Temperature 23.0 °C |
93.7 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 127 J @Temperature 23.0 °C |
93.7 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, all-weld metal, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 127 J @Temperature 23.0 °C |
93.7 ft-lb @Temperature 73.4 °F |
|
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 127 J | 93.7 ft-lb | V Notch |
Haynes Ultimet® alloy, plate, GMAW weld (short) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Charpy Impact | 127 J | 93.7 ft-lb | V Notch |
Haynes Ultimet® alloy, plate, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |